15% off Comfrt — auto-applied at checkout, no code.
Get 15% Off →

TPU Filament Guide: Settings, Hardness and Printing Tips

SUNLU TPU flexible 3D printer filament spool
Image: SUNLU (store.sunlu.com)

Disclosure: We may earn a commission from purchases made through links in this article, at no extra cost to you.

SUNLU logo

SUNLU✓ Offers checked 19 Nov 2026
3% OFFDK26WO527RShow code

3% off select SUNLU collections with our exclusive code

Get this deal →

FREE SHIPPING

Free shipping on SUNLU US orders over $40

Get this deal →

The short answer

TPU is a flexible, rubber-like filament used for parts that need to bend, grip or absorb impact, such as gaskets, bumpers, grips and RC tires. It prints at roughly 210 to 245°C depending on the brand, but it needs slow speeds, little or no retraction and dry filament. Firmer 95A TPU is the easiest place to start; softer grades are harder to feed through an extruder.

TPU at a glance

  • Common 3D printing grades: about 85A to 95A Shore hardness.
  • Nozzle temperature: 190–250°C across the brands we checked.
  • Typical speed: about 20–50 mm/s; high-flow grades list up to 100 mm/s.
  • Drying: 60–70°C for 4–8 hours, depending on the maker.

What TPU is

TPU stands for thermoplastic polyurethane. Prusa’s flexible materials guide describes it as a type of TPE (thermoplastic elastomer) and notes that the main difference between flexible materials is their Shore hardness. Prusa also notes that the softer a filament is, the harder it is to print.

What 95A and 85A mean

Shore hardness is measured by pressing an indenter into the material under a set force (ASTM D2240, as Intertek explains). On the Shore A scale used for soft materials, a lower number means softer and more flexible. A 95A TPU is firm but still flexible; an 85A TPU bends and rebounds more but prints slower and needs more care, according to MatterHackers.

Diagram of the Shore A hardness scale showing 60A, 85A, 90A and 95A
Lower Shore A numbers are softer. Sources: Intertek, Prusa, MatterHackers. Diagram: Hnlsharing.

TPU print settings

Manufacturers publish different ranges, so use your own filament’s data sheet first. Here is what the sources we checked recommend:

SourceNozzleBedSpeedCooling fan
Prusa (generic flex)230–245°C60–75°CAbout 20 mm/s (max 30–40)Off
Polymaker PolyFlex TPU95210–230°C25–60°C30–50 mm/sOn
Polymaker PolyFlex TPU95-HF200–230°C25–50°C30–100 mm/sNot listed in our notes
SUNLU TPU 95A190–230°CNot listedNot listedNot listed
eSUN eTPU-95A220–250°C45–60°CNot listedNot listed

Note the disagreement on part cooling: Prusa recommends keeping it off for flex, while Polymaker lists the fan on for PolyFlex TPU95. Start with your filament maker’s setting and adjust if layers do not bond well.

Chart of TPU nozzle temperature ranges and print speeds from Prusa, Polymaker, SUNLU and eSUN
Nozzle temperature and speed ranges by source (read November 19, 2026). Chart: Hnlsharing.

Why TPU has to print slowly

Because TPU is soft, pushing it hard makes it bend and buckle inside the extruder instead of moving through the nozzle. Prusa recommends loosening the extruder idler, since tightly clamped gears can tangle flexible filament. MatterHackers suggests limiting the slicer’s maximum volumetric speed rather than relying on a single fast print speed.

Direct drive vs Bowden

  • Direct drive extruders keep the filament path short, which makes all TPU grades easier, especially softer ones.
  • Bowden setups can print firmer 95A TPU. MatterHackers calls “Bowden can’t print TPU” a myth, but recommends a tightly guided path and very low or zero retraction.
  • Prusa notes that filament sensors and automatic filament changes may not work reliably with flexible filament.

Retraction and bed adhesion

  • Retraction: Prusa suggests using less, or starting at zero and increasing gradually. MatterHackers calls retraction “often the #1 cause of TPU headaches.”
  • Bed adhesion: TPU can stick too well to smooth or satin PEI. Prusa recommends glue stick as a release layer on those sheets; textured PEI usually needs none. Avoid squishing the first layer too much.

Tip: if your first TPU print strings badly, dry the spool before you change any other setting. Wet TPU strings and pops even with good settings.

Drying TPU

TPU absorbs moisture from the air. Polymaker’s data sheet recommends 70°C for 8 hours for PolyFlex TPU95, and Prusa’s drying table lists 60°C for 4 to 6 hours. Read more in our guide to whether you need a filament dryer.

What TPU is good for, and what it is not

  • Good for: washers, gaskets and light seals, bumpers and impact protection, grips, wearables, RC tires, stamps and shoe soles (Prusa, MatterHackers).
  • Not a good fit: rigid structural parts, high-heat parts and precise snap fits, according to MatterHackers.
  • Trade-offs: slow printing, stringing, weak bridges and overhangs, and supports that are hard to remove (Prusa).

Buying TPU from SUNLU? SUNLU lists TPU 95A at $15.99–$17.99 per 1 kg spool on its US store (minimum order applies on some listings, checked 19 Nov 2026).

See SUNLU deals →

How we researched this

This guide is research-based; we did not print these filaments for this article. On November 19, 2026 we read Prusa’s flexible materials guide, Polymaker’s PolyFlex TPU95 and TPU95-HF data sheets, Intertek on Shore hardness, MatterHackers’ TPU guide, and SUNLU and eSUN product pages.

Frequently asked questions

What is TPU filament?

TPU (thermoplastic polyurethane) is a flexible, rubber-like 3D printing filament and a type of TPE. Common grades for 3D printing range from about 85A to 95A on the Shore A hardness scale, and Prusa notes that TPU can be as soft as around 60A.

What temperature should I print TPU at?

It depends on the brand. Prusa’s generic flex guidance is 230 to 245°C, Polymaker lists 210 to 230°C for PolyFlex TPU95, SUNLU lists 190 to 230°C for its TPU 95A and eSUN lists 220 to 250°C for eTPU-95A. Start in the middle of your filament maker’s range.

How fast can you print TPU?

Slowly compared with PLA. Prusa suggests about 20 mm/s with a maximum around 30 to 40 mm/s for flex, and Polymaker lists 30 to 50 mm/s for PolyFlex TPU95. High-flow grades such as Polymaker TPU95-HF list up to 100 mm/s.

Can you print TPU with a Bowden extruder?

Often yes, especially with firmer 95A TPU, but it is harder. MatterHackers calls “Bowden can’t print TPU” a myth and says a tightly guided filament path matters most; use very low or zero retraction. Softer grades are much easier on a direct drive extruder.

Why does TPU stick so hard to my PEI sheet?

Flexible filaments can bond very strongly to smooth PEI. Prusa recommends a thin layer of glue stick as a separator on smooth or satin PEI; textured PEI sheets usually do not need it.

Does TPU need to be dried?

Yes. TPU absorbs moisture, which causes stringing and popping. Polymaker recommends drying PolyFlex TPU95 at 70°C for 8 hours, and Prusa’s drying table lists 60°C for 4 to 6 hours for TPU. Follow your filament maker’s data sheet.

The bottom line

Start with a 95A TPU, dry it, print slowly with little retraction, and use glue stick on smooth PEI. Once that works, softer grades and high-flow TPU are easier to tune. Always begin with the temperature range on your own spool, since brands differ by up to 40°C.

Ha Ngoc Loc

about the author

Ha Ngoc Loc
Editorial Team

Ha Ngoc Loc is the founder and editor of Hnlsharing. Loc researches each brand from its official product pages, pricing, shipping, return and warranty policies, and from customer reviews on independent platforms such as Trustpilot. Hnlsharing does not buy or test products hands-on, so every review says it is research-based and shows the date its facts were checked. Coupons and deals come from brands and their affiliate programs, and each offer shows the date it was last checked on the brand's site.